HomeNews News Industry Information How to Choose the Right Additive for Powder Coatings?

How to Choose the Right Additive for Powder Coatings?

2026-08-21

Choose a powder coating additive by identifying the defect or performance target, confirming the Resin and curing system, and testing the lowest effective dosage under the real extrusion and curing conditions. An OEM/ODM manufacturer of powder coating Additives should not recommend a product from the defect name alone.

Begin With Evidence, Not Assumptions

“Poor surface” is not a technical diagnosis.

Record what the defect looks like, when it appears and whether it affects every coated part.

Useful evidence includes:

  • Clear photographs

  • Substrate type

  • Pretreatment process

  • Film thickness

  • Extrusion temperature

  • Particle-size distribution

  • Spray settings

  • Oven air temperature

  • Actual metal temperature

  • Cure time

  • Existing formula

Changing an additive before collecting this information may hide the original cause.

Orange Peel: Check Flow and Gel Timing Together

Orange peel can result from poor melt flow, fast gelation, unsuitable viscosity, coarse particles, excessive film thickness or application conditions.

A leveling agent may improve surface smoothness, but the formulator should also review:

  1. Resin melt viscosity

  2. Curing speed

  3. Extrusion dispersion

  4. Powder particle size

  5. Film build

  6. Oven profile

Our additive range includes acrylate-based flow and surface-control products for different powder systems.

Pinholes: Find the Source of the Gas

Pinholes may come from:

  • Porous castings

  • Galvanized substrates

  • Moisture

  • Contaminated Fillers

  • Trapped air

  • Volatile components

  • Excess film thickness

  • Rapid gelation

A degassing agent such as benzoin may help, but it cannot correct oil contamination or severely under-dried raw materials.

Run the same formula on a controlled metal panel and the actual production substrate. If the defect appears only on the production part, the substrate or pretreatment deserves closer attention.

Uneven Gloss: Separate Formulation From Oven Variation

Matting performance depends on resin chemistry, additive distribution, extrusion history, film thickness and cure temperature.

When one section of a large part is glossier than another, measure the actual metal temperature across the workpiece. Uneven heating may be the main cause.

When every panel has the wrong gloss but remains uniform, the matting ratio or formula compatibility is a stronger suspect.

Our outdoor physical matting additive is developed for TGIC systems and specified outdoor matte ranges. That does not mean it should be transferred directly into every HAA or hybrid formulation.

Poor Scratch Resistance: Review the Whole Film

Wax additives can improve slip and reduce surface friction. However, weak scratch performance can also result from under-curing, low crosslink density or unsuitable resin hardness.

Check cure first. A wax should enhance a properly formed film rather than compensate for incomplete crosslinking.

Select the Trial Dosage

An OEM/ODM manufacturer of powder coating additives should provide a recommended starting range, but laboratory validation remains necessary.

A controlled trial can compare:

  • Formula without the additive

  • Low dosage

  • Middle dosage

  • Upper recommended dosage

Keep all other variables constant. Evaluate appearance, gloss, adhesion, impact, bending, hardness, recoating and the specific target property.

Scale Up Carefully

A laboratory mixer and production extruder do not provide identical shear, residence time or temperature history.

During scale-up, monitor:

  • Feed stability

  • Extrudate appearance

  • Extrusion temperature

  • Cooling behaviour

  • Grinding

  • Powder flow

  • Spray performance

  • Cured-film results

Our technical and manufacturing network combines 28 years of powder-coating experience with five production bases across China and Southeast Asia. We support formulation evaluation as well as repeat commercial supply.

Request a Defect-Based Trial Plan

Send one formulation at a time, together with the production evidence and target improvement. We can recommend which variable to test first and what film properties should be checked after the change.

Ask our OEM/ODM manufacturer of powder coating additives for a trial proposal.